The wear resistance of the biomedical low-carbon Co-28Cr-6Mo (wt.-%) alloy is primarily determined by the onset and magnitude of the face-centered cubic to hexagonal close-packed deformation-induced martensitic phase transformation. In metal-on-metal joint bearings, local plastic deformation occurs on the surface and in the subsurface regions. This can cause deformation-assisted structural changes in the materi...