Abstract The objective of this study was to evaluate the effect of the exposure reciprocity law of a multi-wave light-emitting diode (LED) on the light transmittance (LT), depth of cure (DOC) and degree of conversion in-depth (DC) of a bulk fill composite. A bulk fill composite (EvoCeram® bulk fill, Ivoclar Vivadent) was photoactivated using the multi-wave LED (VALO™ Cordless, Ultradent). The LED was previously...
Abstract The purpose of this in vitro study was to evaluate the force decrease of different elastomeric chains after different times: initial, 10 minutes, 1 day, 28 days and after mechanical brushing. Twenty orthodontic elastomeric chains segments were utilized for each commercial brand. Initially, the elastomeric chain of 15mm long were immediate stretched up to 20 mm in an Instron and the force was measured i...
Abstract The aim of this study was to evaluate the effect of 2% chlorhexidine digluconate (CHX) on microtensile bond strength (µTBS) between an adhesive system and under 3 dentin conditions. For that, this study evaluated the adhesive interface at initial, after 6 months and 1 year of storage. Forty-eight human third molars were prepared and randomly divided into 3 groups, according to dentin substrates: sound ...
Abstract This in vitro study aimed to evaluate the gaps length and depth of cure of dual-cure bulk-fill resin composites inserted in box-shaped preparations. Box-shaped preparations (4 mm deep) were made in fifteen human third-molars and divided into three groups according to the resin composites (n=5): Dual-cure bulk-fill BulkEZ (BEZ); Dual-cure bulk-fill HyperFIL (HF); and Tetric Evoceram Bulk-fill (TETRIC), ...
Abstract Camphorquinone is the most conventionally used photoinitiator in Dentistry. Although different alternative photoinitiators have been proposed, no photoinitiator was capable of completely substituting camphorquinone. The combination of photoinitiators has been considered the best alternative. Objectives: To evaluate the effect of combining Norrish type I and II photoinitiators on the cure efficiency of ...
Abstract The present study was evaluated the effect of different light activation and thermocycling methods on the shear bond strength (SBS) and on the adhesive remnant index (ARI) of metal brackets bonded to feldspathic ceramic. Hundred metal brackets were bonded to 20 porcelain cylinders, divided into four groups (n=25) based on light activation and thermocycling processes. The cylinders were etched with 10% ...
Abstract The aim of this study was to evaluate the Streptococcus mutans biofilm influence on the roughness (Ra), gloss (GU), surface hardness (KHN) and flexural strength (FS) of high viscosity bulk fill composites. Filtek Bulk Fill (FBF), Tetric N Ceram Bulk Fill (TNC), X-tra fil Bulk Fill (XF) and Filtek Z350 (FZ) were used. Ten discs of each composite were prepared for Ra, KHN and GU and 20 bars for the FS. A...
Abstract This study evaluated gloss and color changes of esthetic restorative materials subjected to different acidic beverages. Specimens of resin composites (Z350XT (Z350), IPS Empress Direct (ED), Charisma Diamond (CD)) were prepared and the initial surface gloss and color (ΔE) were measured (n=10). Then, the specimens were immersed in 4 mL of each of the different beverages (cranberry juice; Coca-Cola; coff...
Abstract This study to evaluate the effects of different hydrofluoric acid (HF) concentrations and thermal cycling on the shear bond strength (SBS) of brackets to ceramic. Cylinders of ceramic were divided into 10 groups (n=15), according to HF concentrations: 1-1%;2-2.5%;3-5%;4-7.5%;5-10% (storage 24 h); 6-1%;7-2.5%;8-5%;9-7.5%; and, 10-10% (thermal cycling). All cylinders were etched for 60s and received one ...
Abstract The aim of this study was to evaluate Knoop hardness of different shades of a resin cement light-cured directly or through ceramic discs, measured 15 min or 24 h after light exposure, and at different depths. Specimens of a commercial resin cement (Variolink Veneer) in seven shades, were fabricated in an elastomeric mold, covered with a mylar strip, a 0.7 mm thick ceramic disc (IPS e.max Press) was pla...