This work reports the development of porous poly (ε-caprolactone) (PCL)-based intraocular implants, prepared by green supercritical carbon dioxide (scCO2) foaming/mixing method (SFM), to produce implants that degrade faster than typical slow-degrading PCL-based implants. The higher porosities and surface areas of these implants led to faster degradation rates at in vitro accelerated alkaline conditions than low...