Resumo:Novel composite rods were produced by a special braiding technique that involves braiding of polyester yarns around a core of resin-impregnated carbon fibres and subsequent curing. The surface roughness of these braided rods was tailored by replacing one or two simple yarns in the outer-braided layer with braided yarns (produced from 8 simple yarns) and adjusting the take-up velocity. Pull-out tests were carried out to characterize the bond behaviour of these composite rods with cementitious matrix. It was observed that the rod produced with two braided yarns in the outer cover and highest take-up speed was ruptured completely before pull-out, leading to full utilization of its tensile strength, and exhibited 134% higher pull-out force as compared to the rods produced using only simple braiding yarns.
Autores principais:Cunha, Fernando Eduardo Macedo
Outros Autores:Rana, Sohel; Fangueiro, Raúl; Vasconcelos, Graça
Assunto:Composite rods surface tailoring cementitious matrix pull-out test bonding characteristics
Ano:2014
País:Portugal
Tipo de documento:artigo
Tipo de acesso:acesso restrito
Instituição associada:Universidade do Minho
Idioma:inglês
Origem:RepositóriUM - Universidade do Minho
Descrição
Resumo:Novel composite rods were produced by a special braiding technique that involves braiding of polyester yarns around a core of resin-impregnated carbon fibres and subsequent curing. The surface roughness of these braided rods was tailored by replacing one or two simple yarns in the outer-braided layer with braided yarns (produced from 8 simple yarns) and adjusting the take-up velocity. Pull-out tests were carried out to characterize the bond behaviour of these composite rods with cementitious matrix. It was observed that the rod produced with two braided yarns in the outer cover and highest take-up speed was ruptured completely before pull-out, leading to full utilization of its tensile strength, and exhibited 134% higher pull-out force as compared to the rods produced using only simple braiding yarns.